Verschiedene Stahlbearbeitungen
| ISO | Werkstoffe | Chipbreaker | Sorte | vc (m/min) (SFM) | ap (mm) (inch) | f (mm/rev) (IPR) |
|---|---|---|---|---|---|---|
| Kohlenstoffstahl Legierter Stahl | AM3 | ZM3 | 40 – 90 130 – 300 | 0.4 – 2.0 .016 – .080 | 0.05 – 0.2 .002 – .008 | |
| S | 0.1 – 3.0 .004 – .120 | 0.05 – 0.2 .002 – .008 | ||||
| U/U1 | 0.1 – 3.0 .004 – .120 | 0.05 – 0.2 .002 – .008 | ||||
| Schwer zu schneiden Freischneidender rostfreier Stahl | AM3 | 40 – 90 130 – 300 | 0.4 – 2.0 .016 – .080 | 0.05 – 0.2 .002 – .008 | ||
| S | 0.1 – 3.0 .004 – .120 | 0.05 – 0.2 .002 – .008 | ||||
| U/U1 | 0.1 – 3.0 .004 – .120 | 0.05 – 0.2 .002 – .008 | ||||
| Nichteisenmetall | AM3 | 40 – 180 130 – 600 | 0.4 – 2.0 .016 – .080 | 0.05 – 0.2 .002 – .008 | ||
| S | 0.1 – 3.0 .004 – .120 | 0.05 – 0.2 .002 – .008 | ||||
| U/U1 | 0.1 – 3.0 .004 – .120 | 0.05 – 0.2 .002 – .008 |
| Elektronisches Bauteil | |
|---|---|
|
![]() |
|
|
|
|
|
|
|
|
| ZM3 |
1.300 Stück / Ecke
|
| PVD-beschichtetes Hartmetall des Wettbewerbs |
1.000 Stück / Schneide
|
ZM3 konnte eine gleichwertige Oberflächengüte beibehalten und gleichzeitig eine 1,3× längere Standzeit erreichen, dank der hervorragenden Haftfestigkeit der Beschichtung.
| Fall | |
|---|---|
|
![]() |
|
|
|
|
|
|
|
|
| ZM3 |
6.000 Stück und mehr / Ecke |
| PVD-beschichtetes Hartmetall des Wettbewerbs | 150 Stück / Ecke |
ZM3 zeigte eine ca. 40-fach längere Standzeit als der Mitbewerber, unterstützt durch eine hervorragende Haftfestigkeit der Beschichtung und stabile Bauteilabmessungen.
Weitere Informationen zu diesem Produkt finden Sie in unserem Online-E-Katalog, oder laden Sie den Katalog/Produktbericht herunter