车削 – 硬化材料,连续切削
在 HRC55 下,陶瓷的耐磨性优于 CBN 加工。
雨刷类型插入的效果
[ 切削条件 ]
CNGA120412 vc =
100m/min
330 SFM
f =
0.1mm/rev
.004 IPR
ap =
0.5mm
.020 DOC
使用带有 AG 型断屑槽的 ZC7 刀片可以提高表面光洁度,减少因切屑缠结造成的机床停机时间。从而提高了生产率。
[ 切削条件 ]
SCM415 – 渗碳HRC50 vc =
150m/min
500 SFM
f =
0.2mm/rev
.008 IPR
ap =
0.2mm
.008 DOC
| 转角 半径 | DOC (mm) (inch) | 进给 (mm/rev) (IPR) |
|---|---|---|
| R0.4 R .016 | 0.15 .006 | 0.05 ~ 0.08 .002 ~ .003 |
| R0.8 R .031 | 0.3 .012 | 0.08 ~ 0.10 .003 ~ .004 |
| R1.2 R .047 | 0.4 .016 | 0.10 ~ 0.13 .004 ~ .005 |
| R1.6 R .063 | 0.5 .020 | 0.13 ~ 0.16 .005 ~ .006 |
| 圆形刀片 | 2.0 .080 | 0.16 ~ 0.25 .006 ~ .010 |
| 材质分类 | 被加工材料 | 切削油 | 材质 | vc (m/min) (SFM) | ap (mm) (inch) | f (mm/rev) (IPR) |
|---|---|---|---|---|---|---|
| 硬车削精加工 连续 |
DRY/WET | ZC7 | 40 – 200 130 – 660 | 0.1 – 0.7 .004 – .030 | 0.07 – 0.2 .003 – .008 | |
| 轧辊 粗加工车削 |
DRY | HC7 | 90 – 180 300 – 600 | 0.5 – 2.0 .020 – .080 | 0.1 – 0.3 .004 – .012 | |
| 轧辊 粗加工车削(CPM) |
120 – 150 400 – 500 | 0.6 – 2.0 .024 – .080 | 0.1 – 0.3 .004 – .012 |